Unfortunately there are no photos of the masking on the bottom hot coat or any more construction photos as my cameraman wasn't on hand.
But in a nutshell after the bottom was hot coated the board was sanded smooth right back to the cloth in places if needed to ensure a very smooth board prior to gloss coat. Again all the sanding marks would dissapear once the gloss coat goes on. Grits used were 80, 120 and 240.
With the board sanded the pinline was added over the top of the cutlap. One of my favourite bits adding the pinline, it just adds that extra something to a board.
Very careful masking was used on both top and bottom gloss coats as i didn't want any stray resin at this point.
Gloss coat was sanded using 240 upto 600 grit then the board was polished.